EN 12167 Grade CuZn39Pb1 H105

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Hardness, Brinell

20.0 °C

105 [-]

Show Material materials with Hardness, Brinell of 105 [-]

Hardness, Vickers

20.0 °C

110 [-]

Show Material materials with Hardness, Vickers of 110 [-]

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Copper

59 - 60 %

Show Material materials with Copper of 59 - 60 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.8 - 1.6 %

Show Material materials with Lead of 0.8 - 1.6 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %