EN 12167 Grade CuZn36Sn1Pb H100

.XLSX
.PDF
Save

Description

Material CuZn36Sn1Pb (CW712R) is incomparable to a DIN-make. It is used in the form of rods, hollow rods, profiles, wires, forging prematerial and forged parts.

Related Standards

Equivalent Materials

Properties

Mechanical

Hardness, Brinell HB

0 - 100 [-] at 20 °C

Hardness, Vickers HV

0 - 105 [-] at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

61 - 63 %

Sn

1 - 1.5 %

Pb

0.2 - 0.6 %

Fe

0 - 0.1 %

Ni

0 - 0.2 %

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.