EN 12167 Grade CuZn37Pb1Sn1 H120

.XLSX
.PDF
Save

Description

Material CuZn37Pb1Sn1 (CW714R) is incomparable to a DIN-make. It is used in the form of rods and hollow rods, profiles, wires, forging prematerial and forged parts.

Related Standards

Equivalent Materials

Properties

Mechanical

Hardness, Brinell HB

0 - 120 [-] at 20 °C

Hardness, Vickers HV

0 - 125 [-] at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

59 - 61 %

Sn

0.5 - 1 %

Pb

0.4 - 1 %

Fe

0 - 0.1 %

Ni

0 - 0.3 %