EN 12167 Grade CuAl7Si2 R500

.XLSX
.PDF
Save

Description

Material CuAl7Si2 (CW302G) is incomparable to a DIN-make. It is used in the form of bars, profiles, prematerial for forged parts and forged parts.

Related Standards

Equivalent Materials

Properties

Mechanical

Tensile strength Rm

0 - 500 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

250 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

88.55 %

Al

6.3 - 7.6 %

Si

1.5 - 2.2 %

Fe

0 - 0.3 %

Pb

0 - 0.05 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.