EN 12451 Grade CuNi10Fe1Mn soft annealed (+A)

.XLSX
.PDF
Save

Description

The material according this standard is used for seamless, round tubes for heat exchangers, condensers, evaporators and desalination equipment. It can be used for the working in sea water.

Related Standards

Equivalent Materials

Properties

General

Density ρ

8.9 g/cm³ at 20 °C

Mechanical

Elastic modulus E

153 GPa at -253 °C

Show chart

Elongation A

0 - 30 % at 20 °C

Hardness, Vickers HV

75 - 105 [-] at 20 °C

Tensile strength Rm

0 - 290 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

0 - 90 MPa at 20 °C

Thermal

Specific heat capacity cp

0.38 J/(kg·K) at 20 °C

Thermal conductivity λ

50.2 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Ni

9 - 11 %

Fe

1 - 2 %

Mn

0.5 - 1 %

C

0 - 0.05 %

Co

0 - 0.1 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.