General

PropertyTemperatureValue

Density

20.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Hardness, Brinell

20.0 °C

110 - 160 [-]

Show Material materials with Hardness, Brinell of 110 - 160 [-]

Hardness, Vickers

20.0 °C

120 - 170 [-]

Show Material materials with Hardness, Vickers of 120 - 170 [-]

Tensile strength

20.0 °C

410 MPa

Show Material materials with Tensile strength of 410 MPa

Yield strength Rp0.2

20.0 °C

250 MPa

Show Material materials with Yield strength Rp0.2 of 250 MPa

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Copper

59 - 60 %

Show Material materials with Copper of 59 - 60 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.8 - 1.6 %

Show Material materials with Lead of 0.8 - 1.6 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %