ASTM B134 Grade C26000 H01

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Hardness, Rockwell B HRB

40 - 65 [-] at 20 °C

Hardness, Rockwell Superficial 30-T HRB 30-T

43 - 60 [-] at 20 °C

Tensile strength Rm

340 - 530 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

68.5 - 71.5 %

Pb

0.07 %

Fe

0.05 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.