General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 180 GPa Show Material materials with Elastic modulus of 180 GPa |
Elongation | 23.0 °C | 46 % Show Material materials with Elongation of 46 % |
Tensile strength | 23.0 °C | 400 MPa Show Material materials with Tensile strength of 400 MPa |
Yield strength | 23.0 °C | 81 MPa Show Material materials with Yield strength of 81 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K |
Melting point | 1440 °C Show Material materials with Melting point of 1440 °C | |
Specific heat capacity | 23.0 °C | 450 J/(kg·K) Show Material materials with Specific heat capacity of 450 J/(kg·K) |
Thermal conductivity | 23.0 °C | 80 W/(m·K) Show Material materials with Thermal conductivity of 80 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0 - 0.02 % Show Material materials with Carbon of 0 - 0.02 % |
Copper | 0 - 0.25 % Show Material materials with Copper of 0 - 0.25 % |
Iron | 0 - 0.4 % Show Material materials with Iron of 0 - 0.4 % |
Manganese | 0 - 0.35 % Show Material materials with Manganese of 0 - 0.35 % |
Nickel | 99 - 100 % Show Material materials with Nickel of 99 - 100 % |
Silicon | 0 - 0.35 % Show Material materials with Silicon of 0 - 0.35 % |
Sulfur | 0 - 0.01 % Show Material materials with Sulfur of 0 - 0.01 % |