General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.3 g/cm³ Show Material materials with Density of 8.3 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 GPa Show Material materials with Elastic modulus of 120 GPa | |
Elongation | 23.0 °C | 8.1 % Show Material materials with Elongation of 8.1 % | |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 23.0 °C | 730 MPa Show Material materials with Tensile strength of 730 MPa | |
Yield strength | 23.0 °C | 360 MPa Show Material materials with Yield strength of 360 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K |
Melting point | 1040 °C Show Material materials with Melting point of 1040 °C | |
Specific heat capacity | 23.0 °C | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) |
Thermal conductivity | 23.0 °C | 39 W/(m·K) Show Material materials with Thermal conductivity of 39 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % |
Copper | 76.8 - 85 % Show Material materials with Copper of 76.8 - 85 % |
Iron | 2 - 4 % Show Material materials with Iron of 2 - 4 % |
Manganese | 0 - 1.5 % Show Material materials with Manganese of 0 - 1.5 % |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Other | 0 - 0.5 % Show Material materials with Other of 0 - 0.5 % |
Silicon | 0 - 0.25 % Show Material materials with Silicon of 0 - 0.25 % |
Tin | 0 - 0.2 % Show Material materials with Tin of 0 - 0.2 % |
Zinc | 0 - 0.3 % Show Material materials with Zinc of 0 - 0.3 % |