Electrical conductivity σel
1.74E+8 S/m at 20 °C
Density ρ
3 g/cm³ at 20 °C
Elastic modulus E
73 GPa at 20 °C
Elongation A
8.8 % at 20 °C
Tensile strength Rm
470 MPa at 20 °C
Yield strength YS
330 MPa at 20 °C
Coefficient of thermal expansion α
2.3E-5 1/K at 20 °C
Melting point Tm
500 °C
Specific heat capacity cp
870 J/(kg·K) at 20 °C
Thermal conductivity λ
120 W/(m·K) at 20 °C
Element
Weight %
Comment
90.7 - 94.7 %
3.8 - 4.9 %
1.2 - 1.8 %
0.3 - 0.9 %
0 - 0.2 %