General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.8 g/cm³ Show Material materials with Density of 8.8 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 GPa Show Material materials with Elastic modulus of 110 GPa | |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 23.0 °C | 350 MPa Show Material materials with Tensile strength of 350 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K |
Melting point | 960 °C Show Material materials with Melting point of 960 °C | |
Specific heat capacity | 23.0 °C | 380 J/(kg·K) Show Material materials with Specific heat capacity of 380 J/(kg·K) |
Thermal conductivity | 23.0 °C | 77 W/(m·K) Show Material materials with Thermal conductivity of 77 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Copper | 92.9 - 95.5 % Show Material materials with Copper of 92.9 - 95.5 % |
Iron | 0 - 0.1 % Show Material materials with Iron of 0 - 0.1 % |
Lead | 0 - 0.05 % Show Material materials with Lead of 0 - 0.05 % |
Other | 0 - 0.5 % Show Material materials with Other of 0 - 0.5 % |
Phosphorus | 0.03 - 0.35 % Show Material materials with Phosphorus of 0.03 - 0.35 % |
Tin | 4.5 - 5.8 % Show Material materials with Tin of 4.5 - 5.8 % |
Zinc | 0 - 0.3 % Show Material materials with Zinc of 0 - 0.3 % |