UNS C77000 M20

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

130 GPa

Show Material materials with Elastic modulus of 130 GPa at 23.0 °C

23.0 °C

Poisson's ratio

0.32 [-]

Show Material materials with Poisson's ratio of 0.32 [-] at 23.0 °C

23.0 °C

Typical for Wrought Copper Nickel Silver Grade

Tensile strength

480 MPa

Show Material materials with Tensile strength of 480 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K at 23.0 °C

23.0 °C

Melting point

875 - 1135 °C

Show Material materials with Melting point of 875 - 1135 °C

Typical for Wrought Copper Nickel Silver Grade

Specific heat capacity

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

29 W/(m·K)

Show Material materials with Thermal conductivity of 29 W/(m·K) at 23.0 °C

23.0 °C

Chemical properties

Property

Copper

53.5 - 56.5 %

Iron

0 - 0.25 %

Lead

0 - 0.05 %

Manganese

0 - 0.5 %

Nickel

16.5 - 19.5 %

Other

0 - 0.5 %

Zinc

22.7 - 30 %