General
Property | Value | Condition |
---|---|---|
Density | 5.0 g/cm³ Show Material materials with Density of 5.0 g/cm³ | Moderate Strength |
Mechanical
Property | Value | Condition |
---|---|---|
Elastic modulus | 130.0 GPa Show Material materials with Elastic modulus of 130.0 GPa | Moderate Strength |
Elongation | 12.0 % Show Material materials with Elongation of 12.0 % | Moderate Strength |
Tensile strength | 1070.0 MPa Show Material materials with Tensile strength of 1070.0 MPa | Moderate Strength |
Yield strength | 980.0 MPa Show Material materials with Yield strength of 980.0 MPa | Moderate Strength |
Thermal
Property | Value | Condition | Comment |
---|---|---|---|
Coefficient of thermal expansion | 9.6e-06 1/K Show Material materials with Coefficient of thermal expansion of 9.6e-06 1/K | Moderate Strength | |
Melting point | 1550.0 - 1815.0 °C Show Material materials with Melting point of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy | |
Specific heat capacity | 510.0 J/(kg·K) Show Material materials with Specific heat capacity of 510.0 J/(kg·K) | Moderate Strength | |
Thermal conductivity | 6.0 - 11.0 W/(m·K) Show Material materials with Thermal conductivity of 6.0 - 11.0 W/(m·K) | Typical for Titanium Beta Alloy |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 3.0 - 4.0 % Show Material materials with Aluminium of 3.0 - 4.0 % | Moderate Strength |
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % | Moderate Strength |
Chromium | 5.5 - 6.5 % Show Material materials with Chromium of 5.5 - 6.5 % | Moderate Strength |
Hydrogen | 0.02 % Show Material materials with Hydrogen of 0.02 % | Moderate Strength |
Iron | 0.3 % Show Material materials with Iron of 0.3 % | Moderate Strength |
Molybdenum | 3.5 - 4.5 % Show Material materials with Molybdenum of 3.5 - 4.5 % | Moderate Strength |
Nitrogen | 0.03 % Show Material materials with Nitrogen of 0.03 % | Moderate Strength |
Other | 0.4 % Show Material materials with Other of 0.4 % | Moderate Strength |
Oxygen | 0.12 % Show Material materials with Oxygen of 0.12 % | Moderate Strength |
Palladium | 0.04 - 0.08 % Show Material materials with Palladium of 0.04 - 0.08 % | Moderate Strength |
Titanium | 71.0 - 77.0 % Show Material materials with Titanium of 71.0 - 77.0 % | Moderate Strength |
Vanadium | 7.5 - 8.5 % Show Material materials with Vanadium of 7.5 - 8.5 % | Moderate Strength |
Zirconium | 3.5 - 4.5 % Show Material materials with Zirconium of 3.5 - 4.5 % | Moderate Strength |