General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 10 g/cm³ Show Material materials with Density of 10 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 86 GPa Show Material materials with Elastic modulus of 86 GPa | |
Elongation | 23.0 °C | 4.6 % Show Material materials with Elongation of 4.6 % | |
Poisson's ratio | 23.0 °C | 0.37 [-] Show Material materials with Poisson's ratio of 0.37 [-] | Typical for Silver |
Shear modulus | 23.0 °C | 30 GPa Show Material materials with Shear modulus of 30 GPa | Typical for Silver |
Tensile strength | 23.0 °C | 360 MPa Show Material materials with Tensile strength of 360 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.9E-5 1/K | |
Melting point | 780 °C Show Material materials with Melting point of 780 °C | ||
Specific heat capacity | 23.0 °C | 250 J/(kg·K) Show Material materials with Specific heat capacity of 250 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 417 - 428 W/(m·K) Show Material materials with Thermal conductivity of 417 - 428 W/(m·K) | Typical for Silver |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 5E-3 % Show Material materials with Aluminium of 0 - 5E-3 % |
Cadmium | 0 - 0.05 % Show Material materials with Cadmium of 0 - 0.05 % |
Copper | 9 - 10.4 % Show Material materials with Copper of 9 - 10.4 % |
Iron | 0 - 0.05 % Show Material materials with Iron of 0 - 0.05 % |
Lead | 0 - 0.03 % Show Material materials with Lead of 0 - 0.03 % |
Nickel | 0 - 0.01 % Show Material materials with Nickel of 0 - 0.01 % |
Other | 0 - 0.06 % Show Material materials with Other of 0 - 0.06 % |
Phosphorus | 0 - 0.02 % Show Material materials with Phosphorus of 0 - 0.02 % |
Silver | 89.6 - 91 % Show Material materials with Silver of 89.6 - 91 % |
Zinc | 0 - 0.06 % Show Material materials with Zinc of 0 - 0.06 % |