General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 11 g/cm³ Show Material materials with Density of 11 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 GPa Show Material materials with Elastic modulus of 110 GPa | |
Elongation | 23.0 °C | 2.3 % Show Material materials with Elongation of 2.3 % | |
Poisson's ratio | 23.0 °C | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] | Typical for Palladium |
Shear modulus | 23.0 °C | 42 GPa Show Material materials with Shear modulus of 42 GPa | Typical for Palladium |
Tensile strength | 23.0 °C | 310 MPa Show Material materials with Tensile strength of 310 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K | |
Melting point | 1550 °C Show Material materials with Melting point of 1550 °C | ||
Specific heat capacity | 23.0 °C | 240 J/(kg·K) Show Material materials with Specific heat capacity of 240 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 60 - 76 W/(m·K) Show Material materials with Thermal conductivity of 60 - 76 W/(m·K) | Typical for Palladium |
Chemical properties
Property | Value |
---|---|
Other | 0 - 0.2 % Show Material materials with Other of 0 - 0.2 % |
Palladium | 99.8 - 100 % Show Material materials with Palladium of 99.8 - 100 % |