364 Molybdenum Recrystallized

.XLSX
.PDF
Save

Properties

General

Density ρ

10 g/cm³ at 20 °C

Mechanical

Elastic modulus E

330 GPa at 20 °C

Elongation A

12 % at 20 °C

Tensile strength Rm

590 MPa at 20 °C

Yield strength YS

360 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2E-5 1/K at 20 °C

Specific heat capacity cp

250 J/(kg·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Mo

99.2 - 99.5 %

Ti

0.4 - 0.55 %

Zr

0.06 - 0.12 %

O

0.03 %

C

0.01 - 0.04 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.