Nickel 718 Solution Treated And Aged

.XLSX
.PDF
Save

Properties

General

Density ρ

8.3 g/cm³ at 20 °C

Mechanical

Elastic modulus E

200 GPa at 20 °C

Elongation A

35 % at 20 °C

Tensile strength Rm

1230 MPa at 20 °C

Yield strength YS

920 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.3E-5 1/K at 20 °C

Melting point Tm

1260 °C

Specific heat capacity cp

440 J/(kg·K) at 20 °C

Thermal conductivity λ

11 W/(m·K) at 20 °C

Electrical

Electrical conductivity σel

4.23E+8 S/m at 20 °C

Chemical properties

Element

Weight %

Comment

Ni

50 - 55 %

Cr

17 - 21 %

Fe

11.1 - 24.6 %

Nb

4.8 - 5.5 %

Mo

2.8 - 3.3 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.