AISI 1084 Spheroidized And Cold Drawn

.XLSX
.PDF
Save

Description

Equivalent Materials

Properties

General

Density ρ

7.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

210 GPa at 20 °C

Elongation A

12 % at 20 °C

Poisson's ratio ν

0.29 [-] at 20 °C

Typical for High Carbon Steel

Shear modulus G

75 - 80 GPa at 20 °C

Typical for Carbon Steel

Tensile strength Rm

790 MPa at 20 °C

Yield strength YS

610 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.2E-5 1/K at 20 °C

Max service temperature Tmax

500 °C

Typical for Carbon Steel

Melting point Tm

1289 - 1478 °C

Typical for High Carbon Steel

Specific heat capacity cp

450 J/(kg·K) at 20 °C

Electrical

Electrical resistivity ρel

1.43E-7 - 1.74E-7 Ω·m at 20 °C

Typical for Carbon Steel

Chemical properties

Element

Weight %

Comment

Fe

98.1 - 98.6 %

C

0.8 - 0.93 %

Mn

0.6 - 0.9 %

P

0 - 0.04 %

S

0 - 0.05 %

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.