ASTM B617 Spring-Tempered

.XLSX
.PDF
Save

Ashby charts

See where falls on the material property chart for Density against Elastic modulus in your materials selection and design process.

Properties

General

Density ρ

10 g/cm³ at 20 °C

Mechanical

Elastic modulus E

86 GPa at 20 °C

Elongation A

1.2 % at 20 °C

Tensile strength Rm

520 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.9E-5 1/K at 20 °C

Melting point Tm

780 °C

Specific heat capacity cp

250 J/(kg·K) at 20 °C

Electrical

Electrical conductivity σel

4.81E+8 S/m at 20 °C

Chemical properties

Element

Weight %

Comment

Ag

89.6 - 91 %

Cu

9 - 10.4 %

Al

0 - 5E-3 %

Cd

0 - 0.05 %

Fe

0 - 0.05 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.