ASTM B540 Stress Relieved

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

13 g/cm³

Show Material materials with Density of 13 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

120 GPa

Show Material materials with Elastic modulus of 120 GPa

Elongation

23.0 °C

9.2 %

Show Material materials with Elongation of 9.2 %

Poisson's ratio

23.0 °C

0.39 [-]

Show Material materials with Poisson's ratio of 0.39 [-]

Typical for Palladium

Shear modulus

23.0 °C

42 GPa

Show Material materials with Shear modulus of 42 GPa

Typical for Palladium

Tensile strength

23.0 °C

1040 MPa

Show Material materials with Tensile strength of 1040 MPa

Yield strength

23.0 °C

930 MPa

Show Material materials with Yield strength of 930 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K

Melting point

1020 °C

Show Material materials with Melting point of 1020 °C

Specific heat capacity

23.0 °C

240 J/(kg·K)

Show Material materials with Specific heat capacity of 240 J/(kg·K)

Thermal conductivity

23.0 °C

60 - 76 W/(m·K)

Show Material materials with Thermal conductivity of 60 - 76 W/(m·K)

Typical for Palladium

Chemical properties

PropertyValue

Copper

13.5 - 14.5 %

Show Material materials with Copper of 13.5 - 14.5 %

Gold

9.5 - 10.5 %

Show Material materials with Gold of 9.5 - 10.5 %

Other

0 - 0.3 %

Show Material materials with Other of 0 - 0.3 %

Palladium

34 - 36 %

Show Material materials with Palladium of 34 - 36 %

Platinum

9.5 - 10.5 %

Show Material materials with Platinum of 9.5 - 10.5 %

Silver

29 - 31 %

Show Material materials with Silver of 29 - 31 %

Zinc

0.8 - 1.2 %

Show Material materials with Zinc of 0.8 - 1.2 %