Specific Electrical conductivity
1.28E+8 % IACS
Density ρ
8.8 g/cm³ at 20 °C
Elastic modulus E
120 GPa at 20 °C
Elongation A
17 % at 20 °C
Tensile strength Rm
800 MPa at 20 °C
Yield strength YS
660 MPa at 20 °C
Coefficient of thermal expansion α
1.6E-5 1/K at 20 °C
Melting point Tm
870 °C
Specific heat capacity cp
410 J/(kg·K) at 20 °C
Thermal conductivity λ
110 W/(m·K) at 20 °C
Element
Weight %
Comment
96.3 - 98.2 %
1.6 - 1.8 %
0.2 - 0.6 %
0 - 0.2 %
0 - 0.4 %