Properties

General

Density ρ

8.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

120 GPa at 20 °C

Elongation A

14 % at 20 °C

Tensile strength Rm

880 MPa at 20 °C

Yield strength YS

760 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.6E-5 1/K at 20 °C

Melting point Tm

870 °C

Specific heat capacity cp

410 J/(kg·K) at 20 °C

Thermal conductivity λ

110 W/(m·K) at 20 °C

Electrical

Electrical conductivity σel

1.28E+8 S/m at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

96.3 - 98.2 %

Be

1.6 - 1.8 %

Ni

0.2 - 0.6 %

Al

0 - 0.2 %

Fe

0 - 0.4 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.