UNS C19010 TM08

.XLSX
.PDF
Save

Properties

General

Density ρ

8.9 g/cm³ at 20 °C

Mechanical

Elastic modulus E

120 GPa at 20 °C

Tensile strength Rm

560 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.6E-5 1/K at 20 °C

Specific heat capacity cp

390 J/(kg·K) at 20 °C

Thermal conductivity λ

260 W/(m·K) at 20 °C

Electrical

Electrical conductivity σel

2.90E+8 S/m at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

97.3 - 99.04 %

Ni

0.8 - 1.8 %

Si

0.15 - 0.35 %

P

0.01 - 0.05 %

Other

0 - 0.5 %