General

Density ρ

8.4 g/cm³ at 20 °C

Mechanical

Elastic modulus E

230 GPa at 20 °C

Elongation A

14 % at 20 °C

Tensile strength Rm

1370 MPa at 20 °C

Yield strength YS

950 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.3E-5 1/K at 20 °C

Specific heat capacity cp

430 J/(kg·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Co

57.7 - 68.7 %

Cr

26 - 30 %

Mo

5 - 7 %

Al

0.3 - 1 %

La

0.03 - 0.2 %