Customize your search with filters
Do you have any questions?
Electrical conductivity σel
2.09E+8 S/m at 20 °C
Density ρ
3.1 g/cm³ at 20 °C
Elastic modulus E
74 GPa at 20 °C
Elongation A
6.7 % at 20 °C
Tensile strength Rm
460 MPa at 20 °C
Yield strength YS
340 MPa at 20 °C
Coefficient of thermal expansion α
2.2E-5 1/K at 20 °C
Melting point Tm
540 °C
Specific heat capacity cp
860 J/(kg·K) at 20 °C
Thermal conductivity λ
140 W/(m·K) at 20 °C
Element
Weight %
Comment
91.5 - 93.8 %
5.8 - 6.8 %
0.2 - 0.4 %
0.1 - 0.25 %
0.05 - 0.15 %
This material data has been provided by MakeItFrom.com.