General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 3.1 g/cm³ Show Material materials with Density of 3.1 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 71 GPa Show Material materials with Elastic modulus of 71 GPa |
Elongation | 20.0 °C | 1.5 % Show Material materials with Elongation of 1.5 % |
Tensile strength | 20.0 °C | 240 MPa Show Material materials with Tensile strength of 240 MPa |
Yield strength | 20.0 °C | 200 MPa Show Material materials with Yield strength of 200 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.3E-5 1/K |
Melting point | 540 °C Show Material materials with Melting point of 540 °C | |
Specific heat capacity | 20.0 °C | 960 J/(kg·K) Show Material materials with Specific heat capacity of 960 J/(kg·K) |
Thermal conductivity | 20.0 °C | 150 W/(m·K) Show Material materials with Thermal conductivity of 150 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 88.4 - 93.6 % Show Material materials with Aluminium of 88.4 - 93.6 % |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % |
Copper | 3.5 - 4.5 % Show Material materials with Copper of 3.5 - 4.5 % |
Iron | 1 % Show Material materials with Iron of 1 % |
Magnesium | 1.2 - 1.8 % Show Material materials with Magnesium of 1.2 - 1.8 % |
Manganese | 0.35 % Show Material materials with Manganese of 0.35 % |
Nickel | 1.7 - 2.3 % Show Material materials with Nickel of 1.7 - 2.3 % |
Other | 0.15 % Show Material materials with Other of 0.15 % |
Silicon | 0.7 % Show Material materials with Silicon of 0.7 % |
Titanium | 0.25 % Show Material materials with Titanium of 0.25 % |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % |