3/4-Hard AISI 201

Get more information
Contact Matmatch

Chemical composition

Element Weight %
Fe 67.5 — 75.0
Cr 16.0 — 18.0
Mn 5.5 — 7.5
Ni 3.5 — 5.5
Si 0.0 — 1.0
C 0.0 — 0.15
P 0.0 — 0.06
S 0.0 — 0.03

Properties

Electrical

Electrical conductivity [ σel ]

1.45E+7 S/m

General information

Density [ ρ ]

7.70 g/cm³

Mechanical

Elastic modulus [ E ]

200.00 GPa

Elongation [ A ]

14.00 %

Tensile strength [ Rm ]

1390 MPa

Yield strength [ YS ]

1070 MPa

Thermal

Coefficient of thermal expansion [ α ]

1.3E-5 1/K

Specific heat capacity [ cp ]

500.00 J/(kg·K)

Thermal conductivity [ λ ]

15.00 W/(m·K)

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
MakeItFrom, Iron Boar Labs Ltd.
This material data has been provided by MakeItFrom, Iron Boar Labs Ltd.

Download material data

Material data to download as .xlsx and .pdf file.

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MITF138 to find materials similar to 3/4-Hard AISI 201.