AA Standards Grade 3004 H24

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey,MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated Standards

Density

2.72 g/cm³

Show Material materials with Density of 2.72 g/cm³

H24

AA Standards, ASTM B209

2.8 g/cm³

Show Material materials with Density of 2.8 g/cm³

H24

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H24

AA Standards, ASTM B209

Elongation

1.0 %

Show Material materials with Elongation of 1.0 %

H24

AA Standards, ASTM B209

A50

2.0 %

Show Material materials with Elongation of 2.0 %

H24

AA Standards, ASTM B209

A50

2.3 %

Show Material materials with Elongation of 2.3 %

H24

3.0 %

Show Material materials with Elongation of 3.0 %

H24

AA Standards, ASTM B209

A50

4.0 %

Show Material materials with Elongation of 4.0 %

H24

AA Standards, ASTM B209

A50

4.0 %

Show Material materials with Elongation of 4.0 %

H24

AA Standards, ASTM B209

A100

5.0 %

Show Material materials with Elongation of 5.0 %

H24

AA Standards, ASTM B209

A50

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

25.0 - 26.0 GPa

Show Material materials with Shear modulus of 25.0 - 26.0 GPa

Typical for Wrought 3000 Series Aluminium

Tensile strength

220.0 - 265.0 MPa

Show Material materials with Tensile strength of 220.0 - 265.0 MPa

H24

AA Standards, ASTM B209

240.0 MPa

Show Material materials with Tensile strength of 240.0 MPa

H24

Yield strength

170.0 MPa

Show Material materials with Yield strength of 170.0 MPa

H24

AA Standards, ASTM B209

RP02

200.0 MPa

Show Material materials with Yield strength of 200.0 MPa

H24

Thermal

PropertyTemperatureValueConditionRelated Standards

Coefficient of thermal expansion

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

H24

20 °C

2.3899999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3899999999999998e-05 1/K

H24

AA Standards, ASTM B209

100 °C

2.3899999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3899999999999998e-05 1/K

H24

AA Standards, ASTM B209

Melting point

630.0 - 655.0 °C

Show Material materials with Melting point of 630.0 - 655.0 °C

H24

AA Standards, ASTM B209

630.0 °C

Show Material materials with Melting point of 630.0 °C

H24

Specific heat capacity

890.0 J/(kg·K)

Show Material materials with Specific heat capacity of 890.0 J/(kg·K)

H24

Thermal conductivity

160.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 W/(m·K)

H24

163 W/(m·K)

Show Material materials with Thermal conductivity of 163 W/(m·K)

H24

AA Standards, ASTM B209

Electrical

PropertyValueConditionRelated Standards

Electrical conductivity

24000000.0 S/m

Show Material materials with Electrical conductivity of 24000000.0 S/m

H24

AA Standards, ASTM B209

Electrical resistivity

4.17e-08 Ω·m

Show Material materials with Electrical resistivity of 4.17e-08 Ω·m

H24

AA Standards, ASTM B209

Chemical properties

PropertyValueConditionRelated Standards

Aluminium

95.6 - 98.2 %

Show Material materials with Aluminium of 95.6 - 98.2 %

H24

Copper

0.25 %

Show Material materials with Copper of 0.25 %

H24

AA Standards, ASTM B209

Iron

0.70 %

Show Material materials with Iron of 0.70 %

H24

AA Standards, ASTM B209

0.7 %

Show Material materials with Iron of 0.7 %

H24

Magnesium

0.8 - 1.3 %

Show Material materials with Magnesium of 0.8 - 1.3 %

H24

AA Standards, ASTM B209

Manganese

1.0 - 1.5 %

Show Material materials with Manganese of 1.0 - 1.5 %

H24

AA Standards, ASTM B209

Other

0.15 %

Show Material materials with Other of 0.15 %

H24

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %

H24

AA Standards, ASTM B209

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

H24

AA Standards, ASTM B209

Technological properties

Property
Brazing

general: Lötbar mit speziellen Techniken oder bei bestimmten Anwendungen

Corrosion properties

Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere

General machinability

General: poor (O, H32), sufficient (H34, H36, H38)

Workability

general (condition): good (O), acceptable (H32, H34), poor(H36, H38)