Customize your search with filters
Do you have any questions?
Electrical conductivity σel
2.44E+8 S/m at 20 °C
Density ρ
2.8 g/cm³ at 20 °C
Elastic modulus E
69 GPa at 20 °C
Elongation A
1.7 % at 20 °C
Tensile strength Rm
300 MPa at 20 °C
Yield strength YS
250 MPa at 20 °C
Coefficient of thermal expansion α
2.4E-5 1/K at 20 °C
Melting point Tm
630 °C
Specific heat capacity cp
890 J/(kg·K) at 20 °C
Thermal conductivity λ
160 W/(m·K) at 20 °C
Element
Weight %
Comment
95.6 - 98.2 %
1 - 1.5 %
0.8 - 1.3 %
0 - 0.25 %
0 - 0.3 %
This material data has been provided by MakeItFrom.com.