See where AA 3103 H16 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.8 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.3E-5 1/K at 23 °C
Melting point
Tm640 °C
Specific heat capacity
cp890 J/(kg·K) at 23 °C
Thermal conductivity
λ160 W/(m·K) at 23 °C
Electrical conductivity
σel2.30E+7 - 2.90E+7 S/m at 23 °C
Typical for Wrought 3000 Series Aluminium
Electrical resistivity
ρel3.4E-8 - 4.2E-8 Ω·m at 23 °C
Typical for Wrought 3000 Series Aluminium
Element
Weight %
Comment
96.3 - 99.1 %
0.9 - 1.5 %
0 - 0.1 %
0 - 0.1 %
0 - 0.7 %
Workability
Good workability.