AA 3103 H17

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.8 g/cm³

Show Material materials with Density of 2.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

72 GPa

Show Material materials with Elastic modulus of 72 GPa

Elongation

23.0 °C

3.5 %

Show Material materials with Elongation of 3.5 %

Plane-Strain Fracture Toughnes

23.0 °C

22 - 35 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

23.0 °C

25 - 26 GPa

Show Material materials with Shear modulus of 25 - 26 GPa

Typical for Wrought 3000 Series Aluminium

Tensile strength

23.0 °C

180 MPa

Show Material materials with Tensile strength of 180 MPa

Yield strength

23.0 °C

160 MPa

Show Material materials with Yield strength of 160 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

2.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.3E-5 1/K

Melting point

640 °C

Show Material materials with Melting point of 640 °C

Specific heat capacity

23.0 °C

890 J/(kg·K)

Show Material materials with Specific heat capacity of 890 J/(kg·K)

Thermal conductivity

23.0 °C

160 W/(m·K)

Show Material materials with Thermal conductivity of 160 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical conductivity

23.0 °C

2.30E+7 - 2.90E+7 S/m

Show Material materials with Electrical conductivity of 2.30E+7 - 2.90E+7 S/m

Typical for Wrought 3000 Series Aluminium

Electrical resistivity

23.0 °C

3.4E-8 - 4.2E-8 Ω·m

Show Material materials with Electrical resistivity of 3.4E-8 - 4.2E-8 Ω·m

Typical for Wrought 3000 Series Aluminium

Chemical properties

PropertyValue

Aluminium

96.3 - 99.1 %

Show Material materials with Aluminium of 96.3 - 99.1 %

Chromium

0 - 0.1 %

Show Material materials with Chromium of 0 - 0.1 %

Copper

0 - 0.1 %

Show Material materials with Copper of 0 - 0.1 %

Iron

0 - 0.7 %

Show Material materials with Iron of 0 - 0.7 %

Magnesium

0 - 0.3 %

Show Material materials with Magnesium of 0 - 0.3 %

Manganese

0.9 - 1.5 %

Show Material materials with Manganese of 0.9 - 1.5 %

Other

0 - 0.15 %

Show Material materials with Other of 0 - 0.15 %

Silicon

0 - 0.5 %

Show Material materials with Silicon of 0 - 0.5 %

Titanium

0 - 0.1 %

Show Material materials with Titanium of 0 - 0.1 %

Zinc

0 - 0.2 %

Show Material materials with Zinc of 0 - 0.2 %

Zirconium

0 - 0.1 %

Show Material materials with Zirconium of 0 - 0.1 %

Technological properties

Property
Workability

Good workability.