Electrical conductivity σel
2.44E+8 S/m at 20 °C
Density ρ
2.8 g/cm³ at 20 °C
Elastic modulus E
72 GPa at 20 °C
Elongation A
2.3 % at 20 °C
Tensile strength Rm
210 MPa at 20 °C
Yield strength YS
180 MPa at 20 °C
Coefficient of thermal expansion α
2.3E-5 1/K at 20 °C
Melting point Tm
640 °C
Specific heat capacity cp
890 J/(kg·K) at 20 °C
Thermal conductivity λ
160 W/(m·K) at 20 °C
Element
Weight %
Comment
96.3 - 99.1 %
0.9 - 1.5 %
0 - 0.1 %
0 - 0.2 %
0 - 0.1 %
This material data has been provided by MakeItFrom.com.