Electrical conductivity σel
2.55E+8 S/m at 20 °C
Density ρ
2.8 g/cm³ at 20 °C
Elastic modulus E
69 GPa at 20 °C
Elongation A
2.6 % at 20 °C
Tensile strength Rm
190 MPa at 20 °C
Yield strength YS
170 MPa at 20 °C
Coefficient of thermal expansion α
2.4E-5 1/K at 20 °C
Melting point Tm
640 °C
Specific heat capacity cp
900 J/(kg·K) at 20 °C
Thermal conductivity λ
170 W/(m·K) at 20 °C
Element
Weight %
Comment
96 - 99.5 %
0.3 - 0.8 %
0.2 - 0.8 %
0 - 0.4 %
0 - 0.1 %
This material data has been provided by MakeItFrom.com.