See where Pink Sheets Grade 355.0 T51 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.8 g/cm³ at 20 °C
Coefficient of thermal expansion
α2.3E-5 1/K at 20 °C
nominal value between 20°C and the mentioned temperature
Melting point
Tm546 - 621 °C
Specific heat capacity
cp880 J/(kg·K) at 20 °C
Thermal conductivity
λ170 W/(m·K) at 20 °C
unstated value
Electrical conductivity
σel2.49E+7 - 2.49E+8 S/m at 20 °C
Typical/Derived values
Electrical resistivity
ρel4.01E-8 Ω·m at 20 °C
Typical values
Specific Electrical conductivity
43 % IACS
Typical values
Element
Weight %
Comment
90.3 - 94.1 %
4.5 - 5.5 %
1 - 1.5 %
0.4 - 0.6 %
0 - 0.25 %
This material data has been provided by MakeItFrom.com,ASM Handbook Volume 2 Properties and Selection: Nonferrous oys and Special-Purpose Materials,CastAl_Thermal,AluKey.