Electrical conductivity σel
2.44E+8 S/m at 20 °C
Density ρ
2.7 g/cm³ at 20 °C
Elastic modulus E
72 GPa at 20 °C
Elongation A
3.8 % at 20 °C
Tensile strength Rm
130 MPa at 20 °C
Yield strength YS
100 MPa at 20 °C
Coefficient of thermal expansion α
2.2E-5 1/K at 20 °C
Melting point Tm
570 °C
Specific heat capacity cp
970 J/(kg·K) at 20 °C
Thermal conductivity λ
160 W/(m·K) at 20 °C
Element
Weight %
Comment
90.1 - 93.3 %
6.5 - 7.5 %
0.2 - 0.45 %
0 - 0.35 %
0 - 0.25 %