Electrical conductivity σel
3.02E+8 S/m at 20 °C
Density ρ
2.7 g/cm³ at 20 °C
Elastic modulus E
69 GPa at 20 °C
Elongation A
2.9 % at 20 °C
Tensile strength Rm
160 MPa at 20 °C
Yield strength YS
120 MPa at 20 °C
Coefficient of thermal expansion α
2.4E-5 1/K at 20 °C
Melting point Tm
630 °C
Specific heat capacity cp
900 J/(kg·K) at 20 °C
Thermal conductivity λ
200 W/(m·K) at 20 °C
Element
Weight %
Comment
97 - 99.5 %
0.5 - 1.1 %
0 - 0.25 %
0 - 0.3 %
0 - 0.15 %