See where AA 5005 H28 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.7 g/cm³ at 20 °C
Coefficient of thermal expansion
α2.4E-5 1/K at 20 °C
Max service temperature
Tmax150 °C
Typical for Wrought 5000 Series Aluminium
Melting point
Tm630 °C
Specific heat capacity
cp900 J/(kg·K) at 20 °C
Thermal conductivity
λ200 W/(m·K) at 20 °C
Electrical conductivity
σel3.02E+8 S/m at 20 °C
Electrical resistivity
ρel3.3E-8 - 5E-8 Ω·m at 20 °C
Typical for Wrought 5000 Series Aluminium
Element
Weight %
Comment
97 - 99.5 %
0.5 - 1.1 %
0 - 0.1 %
0 - 0.2 %
0 - 0.7 %
Workability
Good workability.
This material data has been provided by MakeItFrom.com.