1/8-Hard AISI 304L

Chemical composition

Element Weight %
Fe 64.874.5
Cr 17.520.0
Ni 8.012.0
Mn 0.02.0
Si 0.01.0
P 0.00.045
C 0.00.03
S 0.00.03


Electrical conductivity, σ
7.54E+7 S/m
General information
Density, ρ
7.80 g/cm³
Elastic modulus, E
200.00 GPa
Elongation, A
35.00 %
Tensile strength, Rm
790.00 MPa
Yield strength, YS
440.00 MPa
Coefficient of thermal expansion, α
1.7E-5 1/K
Melting point, Tm
1400 °C
Specific heat capacity, cp
500.00 J/(kg·K)
Thermal conductivity, λ
16.00 W/(m·K)
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
MakeItFrom, Iron Boar Labs Ltd.
This material data has been provided by MakeItFrom, Iron Boar Labs Ltd.