AA 5049 H11

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

H11

Mechanical

PropertyValueConditionComment

Elastic modulus

71.0 GPa

Show Material materials with Elastic modulus of 71.0 GPa

H11

Elongation

15.0 %

Show Material materials with Elongation of 15.0 %

H11

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Tensile strength

220.0 MPa

Show Material materials with Tensile strength of 220.0 MPa

H11

Yield strength

120.0 MPa

Show Material materials with Yield strength of 120.0 MPa

H11

Thermal

PropertyValueConditionComment

Coefficient of thermal expansion

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

H11

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

620.0 °C

Show Material materials with Melting point of 620.0 °C

H11

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H11

Thermal conductivity

140.0 W/(m·K)

Show Material materials with Thermal conductivity of 140.0 W/(m·K)

H11

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

3.3e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m

Typical for Wrought 5000 Series Aluminium

Chemical properties

PropertyValueCondition

Aluminium

94.7 - 97.9 %

Show Material materials with Aluminium of 94.7 - 97.9 %

H11

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

H11

Copper

0.1 %

Show Material materials with Copper of 0.1 %

H11

Iron

0.5 %

Show Material materials with Iron of 0.5 %

H11

Magnesium

1.6 - 2.5 %

Show Material materials with Magnesium of 1.6 - 2.5 %

H11

Manganese

0.5 - 1.1 %

Show Material materials with Manganese of 0.5 - 1.1 %

H11

Other

0.15 %

Show Material materials with Other of 0.15 %

H11

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

H11

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

H11

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

H11

Technological properties

Property
Workability

Good workability.