General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 71 GPa Show Material materials with Elastic modulus of 71 GPa | |
Elongation | 23.0 °C | 8.1 % Show Material materials with Elongation of 8.1 % | |
Plane-Strain Fracture Toughnes | 23.0 °C | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m | Typical for Wrought 5000 Series Aluminium |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium |
Shear modulus | 23.0 °C | 26 - 26.5 GPa Show Material materials with Shear modulus of 26 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium |
Tensile strength | 23.0 °C | 250 MPa Show Material materials with Tensile strength of 250 MPa | |
Yield strength | 23.0 °C | 160 MPa Show Material materials with Yield strength of 160 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.4E-5 1/K | |
Max service temperature | 150 °C Show Material materials with Max service temperature of 150 °C | Typical for Wrought 5000 Series Aluminium | |
Melting point | 620 °C Show Material materials with Melting point of 620 °C | ||
Specific heat capacity | 23.0 °C | 900 J/(kg·K) Show Material materials with Specific heat capacity of 900 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 140 W/(m·K) Show Material materials with Thermal conductivity of 140 W/(m·K) |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical conductivity | 23.0 °C | 1.80E+7 - 3.10E+7 S/m Show Material materials with Electrical conductivity of 1.80E+7 - 3.10E+7 S/m | Typical for Wrought 5000 Series Aluminium |
Electrical resistivity | 23.0 °C | 3.3E-8 - 5E-8 Ω·m Show Material materials with Electrical resistivity of 3.3E-8 - 5E-8 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 94.7 - 97.9 % Show Material materials with Aluminium of 94.7 - 97.9 % |
Chromium | 0 - 0.3 % Show Material materials with Chromium of 0 - 0.3 % |
Copper | 0 - 0.1 % Show Material materials with Copper of 0 - 0.1 % |
Iron | 0 - 0.5 % Show Material materials with Iron of 0 - 0.5 % |
Magnesium | 1.6 - 2.5 % Show Material materials with Magnesium of 1.6 - 2.5 % |
Manganese | 0.5 - 1.1 % Show Material materials with Manganese of 0.5 - 1.1 % |
Other | 0 - 0.15 % Show Material materials with Other of 0 - 0.15 % |
Silicon | 0 - 0.4 % Show Material materials with Silicon of 0 - 0.4 % |
Titanium | 0 - 0.1 % Show Material materials with Titanium of 0 - 0.1 % |
Zinc | 0 - 0.2 % Show Material materials with Zinc of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |