General
Property | Value | Condition |
---|---|---|
Density | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | H17 |
Mechanical
Property | Value | Condition | Comment |
---|---|---|---|
Elastic modulus | 71.0 GPa Show Material materials with Elastic modulus of 71.0 GPa | H17 | |
Elongation | 2.3 % Show Material materials with Elongation of 2.3 % | H17 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | |
Shear modulus | 26.0 - 26.5 GPa Show Material materials with Shear modulus of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | |
Tensile strength | 290.0 MPa Show Material materials with Tensile strength of 290.0 MPa | H17 | |
Yield strength | 250.0 MPa Show Material materials with Yield strength of 250.0 MPa | H17 |
Thermal
Property | Value | Condition | Comment |
---|---|---|---|
Coefficient of thermal expansion | 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K | H17 | |
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | |
Melting point | 620.0 °C Show Material materials with Melting point of 620.0 °C | H17 | |
Specific heat capacity | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | H17 | |
Thermal conductivity | 140.0 W/(m·K) Show Material materials with Thermal conductivity of 140.0 W/(m·K) | H17 |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 18000000.0 - 31000000.0 S/m Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 94.7 - 97.9 % Show Material materials with Aluminium of 94.7 - 97.9 % | H17 |
Chromium | 0.3 % Show Material materials with Chromium of 0.3 % | H17 |
Copper | 0.1 % Show Material materials with Copper of 0.1 % | H17 |
Iron | 0.5 % Show Material materials with Iron of 0.5 % | H17 |
Magnesium | 1.6 - 2.5 % Show Material materials with Magnesium of 1.6 - 2.5 % | H17 |
Manganese | 0.5 - 1.1 % Show Material materials with Manganese of 0.5 - 1.1 % | H17 |
Other | 0.15 % Show Material materials with Other of 0.15 % | H17 |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | H17 |
Titanium | 0.1 % Show Material materials with Titanium of 0.1 % | H17 |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H17 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |