AA 5049 H28

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

H28

Mechanical

PropertyValueConditionComment

Elastic modulus

71.0 GPa

Show Material materials with Elastic modulus of 71.0 GPa

H28

Elongation

3.5 %

Show Material materials with Elongation of 3.5 %

H28

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Tensile strength

330.0 MPa

Show Material materials with Tensile strength of 330.0 MPa

H28

Yield strength

260.0 MPa

Show Material materials with Yield strength of 260.0 MPa

H28

Thermal

PropertyValueConditionComment

Coefficient of thermal expansion

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

H28

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

620.0 °C

Show Material materials with Melting point of 620.0 °C

H28

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H28

Thermal conductivity

140.0 W/(m·K)

Show Material materials with Thermal conductivity of 140.0 W/(m·K)

H28

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

3.3e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m

Typical for Wrought 5000 Series Aluminium

Chemical properties

PropertyValueCondition

Aluminium

94.7 - 97.9 %

Show Material materials with Aluminium of 94.7 - 97.9 %

H28

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

H28

Copper

0.1 %

Show Material materials with Copper of 0.1 %

H28

Iron

0.5 %

Show Material materials with Iron of 0.5 %

H28

Magnesium

1.6 - 2.5 %

Show Material materials with Magnesium of 1.6 - 2.5 %

H28

Manganese

0.5 - 1.1 %

Show Material materials with Manganese of 0.5 - 1.1 %

H28

Other

0.15 %

Show Material materials with Other of 0.15 %

H28

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

H28

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

H28

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

H28

Technological properties

Property
Workability

Good workability.