Specific Electrical conductivity
2.03E+8 % IACS
Density ρ
2.7 g/cm³ at 20 °C
Elastic modulus E
71 GPa at 20 °C
Elongation A
6.9 % at 20 °C
Tensile strength Rm
260 MPa at 20 °C
Yield strength YS
180 MPa at 20 °C
Coefficient of thermal expansion α
2.4E-5 1/K at 20 °C
Melting point Tm
620 °C
Specific heat capacity cp
900 J/(kg·K) at 20 °C
Thermal conductivity λ
140 W/(m·K) at 20 °C
Element
Weight %
Comment
94.7 - 97.9 %
1.6 - 2.5 %
0.5 - 1.1 %
0 - 0.3 %
0 - 0.1 %