See where AA 5050 H111 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.7 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.4E-5 1/K at 23 °C
Max service temperature
Tmax150 °C
Typical for Wrought 5000 Series Aluminium
Melting point
Tm630 °C
Specific heat capacity
cp900 J/(kg·K) at 23 °C
Thermal conductivity
λ190 W/(m·K) at 23 °C
Electrical conductivity
σel1.80E+7 - 3.10E+7 S/m at 23 °C
Typical for Wrought 5000 Series Aluminium
Electrical resistivity
ρel3.3E-8 - 5E-8 Ω·m at 23 °C
Typical for Wrought 5000 Series Aluminium
Element
Weight %
Comment
96.3 - 98.9 %
1.1 - 1.8 %
0 - 0.1 %
0 - 0.2 %
0 - 0.7 %
Workability
Good workability.
This material data has been provided by MakeItFrom.com.