AA 5052 H14

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

70 GPa

Show Material materials with Elastic modulus of 70 GPa at 23.0 °C

23.0 °C

Elongation

4.6 %

Show Material materials with Elongation of 4.6 % at 23.0 °C

23.0 °C

Plane-Strain Fracture Toughnes

22 - 35 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23.0 °C

23.0 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C

23.0 °C

Typical for Wrought 5000 Series Aluminium

Shear modulus

26 - 26.5 GPa

Show Material materials with Shear modulus of 26 - 26.5 GPa at 23.0 °C

23.0 °C

Typical for Wrought 5000 Series Aluminium

Tensile strength

250 MPa

Show Material materials with Tensile strength of 250 MPa at 23.0 °C

23.0 °C

Yield strength

210 MPa

Show Material materials with Yield strength of 210 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

2.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.4E-5 1/K at 23.0 °C

23.0 °C

Max service temperature

150 °C

Show Material materials with Max service temperature of 150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

610 °C

Show Material materials with Melting point of 610 °C

Specific heat capacity

900 J/(kg·K)

Show Material materials with Specific heat capacity of 900 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

140 W/(m·K)

Show Material materials with Thermal conductivity of 140 W/(m·K) at 23.0 °C

23.0 °C

Electrical

PropertyValueTemperatureComment

Electrical conductivity

1.80E+7 - 3.10E+7 S/m

Show Material materials with Electrical conductivity of 1.80E+7 - 3.10E+7 S/m at 23.0 °C

23.0 °C

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

3.3E-8 - 5E-8 Ω·m

Show Material materials with Electrical resistivity of 3.3E-8 - 5E-8 Ω·m at 23.0 °C

23.0 °C

Typical for Wrought 5000 Series Aluminium

Chemical properties

Property

Aluminium

95.8 - 97.7 %

Chromium

0.15 - 0.35 %

Copper

0 - 0.1 %

Iron

0 - 0.4 %

Magnesium

2.2 - 2.8 %

Manganese

0 - 0.1 %

Other

0 - 0.15 %

Silicon

0 - 0.25 %

Zinc

0 - 0.1 %

Technological properties

Property
Workability

Good workability.