AA 5052 H16

Want to keep this datasheet? Save it now in your required format

Description

Aluminum AA 5052 is a non-heat treatable alloy with excellent finishing qualities. AA 5052 offers better corrosion resistance than most aluminum alloys, especially to salt water and marine atmospheres. This alloy can be readily welded using most common techniques and is in fact offers some of the best welding characteristics of all aluminum alloys.

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

H16

Mechanical

PropertyValueConditionComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H16

Elongation

2.9 %

Show Material materials with Elongation of 2.9 %

H16

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Tensile strength

270.0 MPa

Show Material materials with Tensile strength of 270.0 MPa

H16

Yield strength

240.0 MPa

Show Material materials with Yield strength of 240.0 MPa

H16

Thermal

PropertyValueConditionComment

Coefficient of thermal expansion

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

H16

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

610.0 °C

Show Material materials with Melting point of 610.0 °C

H16

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H16

Thermal conductivity

140.0 W/(m·K)

Show Material materials with Thermal conductivity of 140.0 W/(m·K)

H16

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

3.3e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m

Typical for Wrought 5000 Series Aluminium

Chemical properties

PropertyValueCondition

Aluminium

95.8 - 97.7 %

Show Material materials with Aluminium of 95.8 - 97.7 %

H16

Chromium

0.15 - 0.35 %

Show Material materials with Chromium of 0.15 - 0.35 %

H16

Copper

0.1 %

Show Material materials with Copper of 0.1 %

H16

Iron

0.4 %

Show Material materials with Iron of 0.4 %

H16

Magnesium

2.2 - 2.8 %

Show Material materials with Magnesium of 2.2 - 2.8 %

H16

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

H16

Other

0.15 %

Show Material materials with Other of 0.15 %

H16

Silicon

0.25 %

Show Material materials with Silicon of 0.25 %

H16

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

H16

Technological properties

Property
Workability

Good workability.