AA 5083 H14

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where AA 5083 H14 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.7 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

71 GPa at 20 °C

Show 5000 Series materials with Elastic modulus of 71 GPa at 20 °C

Elongation

A

3.5 % at 20 °C

Show 5000 Series materials with Elongation of 3.5 % at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 5000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 5000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 5000 Series Aluminium

Shear modulus

G

26 - 26.5 GPa at 20 °C

Show 5000 Series materials with Shear modulus of 26 - 26.5 GPa at 20 °C

Typical for Wrought 5000 Series Aluminium

Tensile strength

Rm

360 MPa at 20 °C

Show 5000 Series materials with Tensile strength of 360 MPa at 20 °C

Yield strength

YS

300 MPa at 20 °C

Show 5000 Series materials with Yield strength of 300 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.4E-5 1/K at 20 °C

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

580 °C

Specific heat capacity

cp

900 J/(kg·K) at 20 °C

Thermal conductivity

λ

120 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

1.68E+8 S/m at 20 °C

Electrical resistivity

ρel

3.3E-8 - 5E-8 Ω·m at 20 °C

Typical for Wrought 5000 Series Aluminium

Chemical properties

Element

Weight %

Comment

Al

92.4 - 95.6 %

Mg

4 - 4.9 %

Mn

0.4 - 1 %

Cr

0.05 - 0.25 %

Cu

0 - 0.1 %

More

Technological properties

Workability

Good workability.

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.