Description

Aluminium 5083 is known for exceptional performance in extreme environments. 5083 is highly resistant to attack by both seawater and industrial chemical environments. Alloy 5083 also retains exceptional strength afterwelding. It has the highest strength of the non-heat treatable alloys but is not recommended for use in temperatures in excess of 65°C.

Related Standards

Equivalent Materials

Ashby charts

See where BS EN 573-3 Grade 5083 H321 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.65 - 2.7 g/cm³ at 20 °C

Dimension

Dimensions

Wanddicke

Mechanical

Elastic modulus

E

71 - 72 GPa at 20 °C

Elongation

A

13 % at 20 °C

Elongation A50

A50

12 % at 20 °C

Hardness, Vickers

HV

95 [-] at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Typical for Wrought 5000 Series Aluminium

Shear modulus

G

26 - 26.5 GPa at 20 °C

Typical for Wrought 5000 Series Aluminium

Shear strength

τ

185 MPa at 20 °C

Tensile strength

Rm

305 - 385 MPa at 20 °C

Yield strength

YS

240 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

215 - 240 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.4E-5 - 2.5E-5 1/K at 20 °C

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

570 - 580 °C

Specific heat capacity

cp

900 J/(kg·K) at 20 °C

Thermal conductivity

λ

120 - 121 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

1.68E+8 S/m at 20 °C

Electrical resistivity

ρel

5.8E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Al

92.4 - 95.6 %

Balance

Mg

4 - 4.9 %

Mn

0.4 - 1 %

Cr

0.05 - 0.25 %

Cu

0 - 0.1 %

More

Technological properties

Application areas

Ship building, Rail cars, Vehicle bodies, Tip truck bodies, Mine skips and cages, Pressure vessels

Brazing

general: no brazing is known or developed

Corrosion properties

Stress corrosion cracking: kein Schadensfall im Betrieb und bei Labortests (O, H321, H116), kein Schadensfall im Betrieb, eingeschränkte Schäden bei den Labortests (H111), general: very good, without protection in industrial or seawater atmosphere

General machinability

General: poor

Workability

general (condition): acceptable (O), poor(H321, H116, H111)

This material data has been provided by Righton Blackburns,MakeItFrom.com,AluKey.