Specific Electrical conductivity
1.86E+8 % IACS
Density ρ
2.7 g/cm³ at 20 °C
Elastic modulus E
70 GPa at 20 °C
Elongation A
3.5 % at 20 °C
Tensile strength Rm
310 MPa at 20 °C
Yield strength YS
260 MPa at 20 °C
Coefficient of thermal expansion α
2.4E-5 1/K at 20 °C
Melting point Tm
590 °C
Specific heat capacity cp
900 J/(kg·K) at 20 °C
Thermal conductivity λ
130 W/(m·K) at 20 °C
Element
Weight %
Comment
94.4 - 96.8 %
3.1 - 3.9 %
0.15 - 0.35 %
0 - 0.1 %
0 - 0.4 %