AA 1060 H112

.XLSX
.PDF
Save

Description

Primary standard name

Properties

General

Density ρ

2.7 g/cm³ at 20 °C

Mechanical

Elastic modulus E

69 GPa at 20 °C

Elongation A

18 % at 20 °C

Elongation A50 A50

10 - 25 % at 20 °C

Tensile strength Rm

60 - 75 MPa at 20 °C

Yield strength YS

17 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

15 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.4E-5 1/K at 20 °C

Melting point Tm

650 °C

Specific heat capacity cp

900 J/(kg·K) at 20 °C

Thermal conductivity λ

230 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

99.6 - 100 %

Fe

0.35 %

Si

0.25 %

Zn

0.05 %

V

0.05 %

More

This material data has been provided by MakeItFrom.com and AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Do you have any questions?

Contact our Material Scientists